fire bricks for sale Fused cast AZS block for glass industry
Refractory bricks Fused cast AZS Castable Refractory Arch crown Refractories brick for glass kiln oven furnace
Types of Refractory bricks Refractory company Fused cast AZS 1711 for glass industry
Physical and chemical index for Types of Refractory bricks
Item | Behaviors | |||
AZS-33# ER 1681 | AZS-36# ER 1685 | AZS-41# ER 1711 | ||
Chemical Composition | Al2O3 | ≥50.00 | ≥49.00 | ≥45.00 |
ZrO2 | ≥32.50 | ≥35.50 | ≥40.50 | |
SiO2 | ≤15.50 | ≤13.50 | ≤13.00 | |
Na2O+K2O | ≤1.30 | ≤1.35 | ≤1.30 | |
Bulk density g/cm3 | ≥3.75 | ≥3.85 | ≥4.00 | |
Apparent Porosity % | ≤1.2 | ≤1.0 | ≤1.2 | |
Cold Crushing Strength Mpa | ≥300 | ≥300 | ≥300 | |
Exudation Temperature of Glass Phase | ≥1400 | ≥1400 | ≥1410 | |
Bubble Separation Ratio(1300°C×10h) | ≤1.2 | ≤1.0 | ≤1.0 | |
Anti-corrosion rate of glass liquid 1500°C×36h (mm/24h)% | ≤1.4 | ≤1.3 | ≤1.2 | |
--Apparent density (g/cm3) | PT(RN RC N) | ≥3.50 | ≥3.50 | ≥3.70 |
ZWS(RR EVF EC ENC) | ≥3.65 | ≥3.70 | ≥3.90 | |
WS( RT VF EPIC FVP DCL) | ≥3.75 | ≥3.8 | ≥4.00 |